Seal Off Repair
This repair was done on the seal off of a mold where inserts have worn out. Minimal weld was added to the molding surface allowing for less downtime and machining.
Modification on Mold Component
Modifications to molds such as new details can be built up with precision. We have the metallurgical knowledge and heating resources to ensure durable welds. Customers are encouraged to send CAD drawings to improve accuracy and precision of build-ups.
Parting Line Edge Repair
Damaged parting line edges can be welded with extreme precision. On this 420ss spoon mold, the parting line was rebuilt without damaging the polished molding surface.
Core Pin Build-up
Core pins vary in size and commonly wear out. The minimal heat affected zone from laser welding allows for various build-ups without distorting the core.
Beryllium Copper Micro TIG Weld Detail Build-up
Beryllium Copper is a non- ferrous alloy that we specialize in welding. We are able to perform large or micro TIG welding repairs with great precision.
A2, M2, and D2 Welding Capabilites
S7 and D2 tool steels are commonly used to make side actions. We are able to deposit minimal pads to shim parts to spec.
Unscrewing Core Repair
We are able to repair unscrewing cores without damaging the microscopic threads or distorting the core.
Beryllium Copper Laser Welded False Bottom
Our new 450F Fiber Laser has exceptional Beryllium Copper welding capabilities. Exemplified in this image is a false bottom measuring 1/2” deep, adding .060” per side of material without distortion.
Edge Build Up
Microscopic razor edges can be repaired with the utmost precision; minimal deposits without undercuts or voids.
Large Mold Laser Repair Using Tilting Optics
Parting Line Modification